应用激光, 2011, 31 (6): 456, 网络出版: 2012-01-05   

TC4钛合金光纤激光焊接工艺研究

Experimental Study on Fibre Laser Welding of Titanium Alloy TC4
作者单位
1 北京工业大学激光工程研究院,北京 100124
2 中国兵器装备研究院,北京 100089
摘要
采用 6 kW光纤激光器焊接 5 mm厚 TC4钛合金,试验研究了焊接工艺参数对焊缝成形的影响,分析了焊接接头微观组织和硬度,测试了室温下焊缝的力学性能。研究结果表明: 光纤激光焊接 5 mm厚钛合金,能够得到成形良好、无裂纹和气孔的焊接接头。接头各区域的显微硬度均高于母材,焊缝抗拉强度与母材相当。
Abstract
A fibre laser was used to weld titanium alloy TC4 witha thickness of 5mm. The effect of parameters on weld profiles, weldmicrostructure and joint mechanical properties was studied experimentally. The results show that weld free of cracks and pores can beobtained. It is found that the micro-hardness of the weld is higher than that of the substrate and the tensile strength is equivalence tothat of the substrate.

杨攀, 徐洁洁, 杨武雄, 肖荣诗, 张文栓, 唐湘燕. TC4钛合金光纤激光焊接工艺研究[J]. 应用激光, 2011, 31(6): 456. Yang Pan, Xu Jiejie, Yang Wuxiong, Xiao Rongshi, Zhang Wenshuan, Tang Xiangyan. Experimental Study on Fibre Laser Welding of Titanium Alloy TC4[J]. APPLIED LASER, 2011, 31(6): 456.

本文已被 1 篇论文引用
被引统计数据来源于中国光学期刊网
引用该论文: TXT   |   EndNote

相关论文

加载中...

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!