CO2激光叠焊不锈钢压力容器的工艺研究

The Process Study of CO2 Laser Stitch Welding Stainless Steel Pressure Vessel
作者单位
1 江苏大学机械学院, 江苏 镇江 212000
2 上海团结普瑞玛激光设备有限公司, 上海 201111
摘要
介绍了激光叠焊幅面为2.4 m×1.2 m, 厚度为1.2 mm的不锈钢板式热交换器的焊接要求和焊接工艺。板式热交换器属压力容器, 因此焊接质量有严格的要求, 针对大幅面不锈钢的尺寸大和易变形等特点, 采取先点焊, 再焊边框, 最后焊内部小圆的工艺流程。点焊有效地控制了焊接过程中变形问题, 并有效地消除了上下板材的间隙问题。内部圆采用了不闭合焊接的处理方法, 显著地减少了气孔现象。对实际焊接后的板材进行耐压试验表明, 采用新焊接工艺的成品件可以承受110 MPa的压力。
Abstract
This paper introduces the welding requirement and welding processes in the laser stitch welding format 2.4 m×1.2 m stainless steel sheet in the thickness 1.2 mm. For easy welding deformation of large-size stainless steel sheet. The spot welding should be taken at first, then welding edges, and finally welding inner circles in order .to prevent deformation .The spot welding is available effectively to control the deformation,and to eliminate the gap between two plates. The inner circles are not closed to reduce efficently the pore phenomenon.The actual sample test of the welded steel plates shows that can withstand 110 MPa.

王晓波, 罗敬文, 张永康. CO2激光叠焊不锈钢压力容器的工艺研究[J]. 应用激光, 2012, 32(3): 198. Wang Xiaobo, Luo Jingwen, Zhang Yongkang. The Process Study of CO2 Laser Stitch Welding Stainless Steel Pressure Vessel[J]. APPLIED LASER, 2012, 32(3): 198.

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!