Recent progress of laser performance in Nd-doped yttrium lanthanum oxide transparent ceramics Download: 647次

Author Affiliations
Abstract
Nd0.02Y1.78La0.2O3 transparent ceramic is fabricated by conventional ceramic sintering process. The transparent ceramic has excellent spectroscopic properties, with the absorption cross section of 1.53×10-20 cm2 and broad full width at half maximum (FWHM) of about 8 nm at 806 nm, the emission cross section of 3.57×10-20 cm2 at 1 078 nm, and the decay lifetime of 232 \mu s. For Nd0.02Y1.78La0.2O3 ceramic laser, a maximum continuous wave (CW) laser output power of 1.38 W with a slope efficiency of 22.9% is obtained at 1 079 nm under an 808 nm diode pump.

Qiuhong Yang, Shenzhou Lu, Haojia Zhang, Qing Wang, Zhiyi Wei, Zhiguo Zhang. Recent progress of laser performance in Nd-doped yttrium lanthanum oxide transparent ceramics[J]. Chinese Optics Letters, 2012, 10(s2): S21417.

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!