摘要
为了得到红外激光在微热管铜基板表面刻蚀复合沟槽的过程中,不同激光工艺参量(激光重复频率、扫描速率、扫描次数)对复合沟槽尺寸和形貌的影响规律,采用单因素实验法进行了红外激光刻蚀微热管复合沟槽的工艺实验研究,确定了使用1064nm波长红外光纤激光器刻蚀微热管复合沟槽的合理工艺参量。结果表明,当激光重复频率为40kHz、扫描速率为150mm/s、扫描次数为25次时,红外激光刻蚀的复合沟槽能为微热管工质的回流提供较大的毛细压力。该研究对提高沟槽式微热管的传热性能具有参考意义。
Abstract
In order to find the effects of different process parameters(laser repetition frequency, laser scanning velocity, laser scanning times) on the dimension and the morphology of composite grooves during laser etching of surface composite grooves on micro heat pipe, a series of experiments were carried out by single factor experimental method. The reasonable process parameters of 1064nm wavelength fiber laser were confirmed. The experimental results show that, under the conditions of 40kHz laser repetition frequency, 150mm/s laser scanning velocity and 25 laser scanning times, composite grooves can provide larger capillary pressure for liquid reflux in micro heat pipe. This study is of great significance to improve the heat transfer performance of grooved micro heat pipes.

杨旸, 魏昕, 谢小柱, 胡伟, 李成彬. 红外激光刻蚀微热管复合沟槽的工艺研究[J]. 激光技术, 2018, 42(2): 276. YANG Yang, WEI Xin, XIE Xiaozhu, HU Wei, LI Chengbin. Study on etching process of composite grooves on micro heat pipes with infrared laser[J]. Laser Technology, 2018, 42(2): 276.

本文已被 2 篇论文引用
被引统计数据来源于中国光学期刊网
引用该论文: TXT   |   EndNote

相关论文

加载中...

关于本站 Cookie 的使用提示

中国光学期刊网使用基于 cookie 的技术来更好地为您提供各项服务,点击此处了解我们的隐私策略。 如您需继续使用本网站,请您授权我们使用本地 cookie 来保存部分信息。
全站搜索
您最值得信赖的光电行业旗舰网络服务平台!