17-4PH不锈钢表面激光熔覆Stellite6涂层组织及耐水蚀性能
任超, 李铸国, 疏达, 赵文雨, 杨仁杰, 王朋, 叶建水. 17-4PH不锈钢表面激光熔覆Stellite6涂层组织及耐水蚀性能[J]. 中国激光, 2017, 44(4): 0402010.
Ren Chao, Li Zhuguo, Shu Da, Zhao Wenyu, Yang Renjie, Wang Peng, Ye Jianshui. Microstructure and Water Erosion Resistance Property of Stellite6 Coating by Laser Cladding on 17-4PH Stainless Steel Surface[J]. Chinese Journal of Lasers, 2017, 44(4): 0402010.
[1] Wang J, Zou H, Li C, et al. The effect of microstructural evolution on hardening behavior of type 17-4PH stainless steel in long-term aging at 350 ℃[J]. Materials Characterization, 2006, 57(4): 274-280.
[2] Raj S V, Ghosn L J, Lerch B A, et al. Mechanical properties of 17-4PH stainless steel foam panels[J]. Materials Science and Engineering: A, 2007, 456(1): 305-316.
[3] 刘志江, 刘向民, 李连相. 近年我国大型汽轮机末级长叶片的冲蚀损伤[J]. 动力工程, 2003, 23(1): 2201-2204.
Liu Zhijiang, Liu Xiangmin, Li Lianxiang. Erosion damage of last stage long blade of large steam turbine in China in recent years[J]. Power Engineering, 2003, 23(1): 2201-2204.
[4] Shepeleva L, Medres B, Kaplan W D, et al. Laser induced Cu/alumina bonding: Microstructure and bond mechanism[J]. Surface and Coatings Technology, 2000, 125(1): 40-44.
[5] Oakley S Y, Nowell D. Prediction of the combined high-and low-cycle fatigue performance of gas turbine blades after foreign object damage[J]. International Journal of Fatigue, 2007, 29(1): 69-80.
[6] 朱蓓蒂, 张之栋. 汽轮机末级叶片的激光熔覆研究[J]. 中国激光, 1994, 21(6): 526-529.
[7] 王东生, 田宗军, 沈理达, 等. 激光熔覆技术研究现状及其发展[J]. 应用激光, 2012, 32(6): 538-544.
[8] 李养良, 金海霞, 白小波, 等. 激光熔覆技术的研究现状与发展趋势[J]. 热处理技术与装备, 2009, 30(4): 1-5.
Li Yangliang, Jin Haixia, Bai Xiaobo, et al. Research status and development trend of laser cladding technology[J]. Heat Treatment Technology and Equipment, 2009, 30(4): 1-5.
[9] Qiao Y F, Fischer T E, Dent A. The effects of fuel chemistry and feedstock powder structure on the mechanical and tribological properties of HVOF thermal-sprayed WC-Co coatings with very fine structures[J]. Surface and Coatings Technology, 2003, 172(1): 24-41.
[10] D′Oliveira A S C, da Silva P S C, Vilar R M. Microstructural features of consecutive layers of Stellite 6 deposited by laser cladding[J]. Surface and Coatings Technology, 2002, 153(2): 203-209.
[11] 段晓溪, 高士友, 顾勇飞, 等. 激光熔覆316L+SiC的强化机制和摩擦磨损性能研究[J]. 中国激光, 2016, 43(1): 0103004.
[12] 徐金涛, 李 安, 刘 栋, 等. 激光熔覆 Cr3Si/γ多相涂层耐蚀性和耐磨性研究[J]. 中国激光, 2016, 43(3): 0303006.
[13] 秦承鹏, 郑玉贵. 17-4PH 不锈钢表面激光熔覆钴基合金涂层的空蚀行为研究[J]. 腐蚀科学与防护技术, 2011, 23(3): 209-213.
Qin Chengpeng, Zheng Yugui. Cavitation erosion behavior of a laser clad Co-based alloy on 17-4PH stainless steel[J]. Corrosion Science and Protection Technology, 2011, 23(3): 209-213.
[14] 杨玉玲, 董丹阳. 材料的激光表面改性技术及应用[M]. 北京: 化学工业出版社, 2013: 72-76.
Yang Yuling, Dong Danyang. Laser surface modification technology and application of Materials[M]. Beijing: Chemical Industry Press, 2013: 72-76.
[15] 王志会, 王华明, 刘 栋. 激光增材制造 AF1410 超高强度钢组织与力学性能研究[J]. 中国激光, 2016, 43(4): 0403001.
[16] Gholipour A, Shamanian M, Ashrafizadeh F. Microstructure and wear behavior of stellite6 cladding on 17-4PH stainless steel[J]. Journal of Alloy and Compounds, 2011, 509(14): 4905-4909.
[17] 王明瑜. B2 模具钢激光熔覆层微观组织与疲劳性能的研究[D]. 长春: 吉林大学, 2015: 25-26.
Wang Mingyu. Study on the microstructure and fatigue properties of B2 mould steel laser cladding layer[D]. Changchun: Jilin University, 2015: 25-26.
[18] Woodford D A. Cavitation-erosion-lnduced phase transformations in alloys[J]. Metallurgical Transactions, 1972, 3(5): 1137-1145.
任超, 李铸国, 疏达, 赵文雨, 杨仁杰, 王朋, 叶建水. 17-4PH不锈钢表面激光熔覆Stellite6涂层组织及耐水蚀性能[J]. 中国激光, 2017, 44(4): 0402010. Ren Chao, Li Zhuguo, Shu Da, Zhao Wenyu, Yang Renjie, Wang Peng, Ye Jianshui. Microstructure and Water Erosion Resistance Property of Stellite6 Coating by Laser Cladding on 17-4PH Stainless Steel Surface[J]. Chinese Journal of Lasers, 2017, 44(4): 0402010.