Inconel X-750镍基合金激光喷丸抗热腐蚀性能及机理
[1] 杨延清, 罗 贤, 黄 斌, 等. Inconel X-750高温合金的组织变化[J]. 材料热处理学报, 2007, 28(S1): 1-4.
Yang Yanqing, Luo Xian, Huang Bin, et al. Microstructure of Inconel X-750 superalloy[J]. Transactions of Materials and Heat Treatment, 2007, 28(S1): 1-4.
[2] 王会阳, 安云岐, 李承宇, 等. 镍基高温合金材料的研究进展[J]. 材料导报, 2011, 25(S2): 482-486.
Wang Huiyang, An Yunqi, Li Chengyu, et al. Research progress of Ni-based superalloys[J]. Materials Review, 2011, 25(S2): 482-486.
[3] 隆小庆. 燃气涡轮发动机高温部件热腐蚀化学反应机理的探讨[J]. 中国民航学院学报, 1994, 12(1): 45-53.
Long Xiaoqing. Chemical reaction mechanism of hot corrosion in high temperature parts of gas turbine engine[J]. Journal of Civil Aviation Institute of China, 1994,12(1): 45-53.
[4] 赵德孜. 海洋环境下燃气轮机涡轮叶片的热腐蚀与防护[J]. 装备环境工程, 2011, 8(5): 100-103.
Zhao Dezi. Hot corrosion and protection of gas turbine blade in marine environment[J]. Equipment Environmental Engineering, 2011, 8(5): 100-103.
[5] 娄学明, 孙文儒, 郭守仁, 等. IN718高温合金热腐蚀行为及其对力学性能的影响[J]. 稀有金属材料与工程, 2008, 37(2): 259-263.
Lou Xueming, Sun Wenru, Guo Shouren, et al. Hot corrosion behavior of IN718 alloy and its effect on mechanical properties[J]. Rare Metal Materials and Engineering, 2008, 37(2): 259-263.
[6] 宁礼奎. 四种镍基高温合金的抗热腐蚀性能研究[D]. 大连: 大连理工大学, 2009.
Ning Likui. Investigation on the hot corrosion resistance of four Ni-based superalloys[D]. Dalian: Dalian University of Technology, 2009.
[7] 黄 舒, 盛 杰, 周建忠, 等. IN718镍基合金激光喷丸微观组织特性及其高温稳定性[J]. 稀有金属材料与工程, 2016, 45(12): 3284-3289.
Huang Shu, Sheng Jie, Zhou Jianzhong, et al. Microstructure characteristics and high-temperature performance of laser peened IN718 Nickel-based alloy[J]. Rare Metal Materials and Engineering, 2016, 45(12): 3284-3289.
[8] Sheng J, Huang S, Zhou J Z, et al. Effects of warm laser peening on the elevated temperature tensile properties and fracture behavior of IN718 nickel-based superalloy[J]. Engineering Fracture Mechanics, 2017, 169: 99-108.
[9] Lu J Z, Qi H, Luo K Y, et al. Corrosion behaviour of AISI 304 stainless steel subjected to massive laser shock peening impacts with different pulse energies[J]. Corrosion Science, 2014, 80: 53-59.
[10] Hua Y Q, Bai Y C, Ye Y X, et al. Hot corrosion behavior of TC11 titanium alloy treated by laser shock processing[J]. Applied Surface Science, 2013, 283: 775-780.
[11] Devaux D, Fabbro R, Tollier L, et al. Generation of shock-waves by laser-induced plasma in confined geometry[J]. Journal of Applied Physics, 1993, 74(4): 2268-2273.
[12] 隆小庆. 航空发动机高温部件热腐蚀机理的探讨[J]. 全面腐蚀控制, 2003, 17(2): 9-13.
Long Xiaoqing. Mechanism of hot corrosion in high temperature parts of aeroengine[J]. Total Corrosion Control, 2003, 17(2): 9-13.
[13] 王长雨. 压铸镁合金双面激光冲击强化残余应力和拉伸性能研究[D]. 镇江: 江苏大学, 2016.
Wang Changyu. Research on residual stress and tensile properties of die casting magnesium alloy during two-sided laser shock processing[D]. Zhenjiang: Jiangsu University, 2016.
[14] 周建忠, 杨小东, 黄 舒, 等. 双面激光喷丸强化ZK60镁合金的残余应力数值研究[J]. 中国激光, 2010, 37(7): 1850-1855.
[15] 章海峰, 黄 舒, 盛 杰, 等. 激光喷丸IN718镍基合金残余应力高温松弛及晶粒演变特征[J]. 中国激光, 2016, 43(2): 0203008.
杨颖秋, 周建忠, 盛杰, 陈松玲, 黄舒, 孟宪凯, 杨祥伟. Inconel X-750镍基合金激光喷丸抗热腐蚀性能及机理[J]. 光学学报, 2017, 37(6): 0614005. Yang Yingqiu, Zhou Jianzhong, Sheng Jie, Chen Songling, Huang Shu, Meng Xiankai, Yang Xiangwei. Hot-Corrosion-Resistance Property and Mechanism of Inconel X-750 Nickel-Based Alloy Processed by Laser Peening[J]. Acta Optica Sinica, 2017, 37(6): 0614005.